Problems, Causes & Solutions In Using The ZING Hard Floor Care System!


Problem



Cause

Solution
Finish is Flaking Off the Floor

Using an incorrect pad.

Using hot water when mopping

Using incorrect finish or incorrect ZING Floor Coating

Use ZING Time Saver Hair Pad for all burnishing.

Use cold water only.

Use ZING Floor Coating + Plus when burnishing often.

Discoloration

Not dust mopping often enough.

Dirty dust mop.

Using hot water when mopping.

Not using ZING Floor Prep often enough.

 

Treat dust mop with ZING Dust Control & mop 1 or 2 times daily.

Clean out dust mop using a piece of used stripping pad by rubbing the surface of mop from top to bottom until clean. Treat again with ZING Dust Control.

Use cold water only.

Use ZING Floor Prep on all high traffic areas at least once per week.

Powdering

Not using a buffable finish or ZING Floor Coating.

Using an incorrect burnishing pad.

Using restoration products.

Not dust mopping often enough.

Dry burnishing.

Using a propane burnisher or finish not intended for a propane machine.

Applying the 2nd coat of of finish before the 1st coat is dry.

Recoating after excessive burnishing.

Finish was frozen, then thawed.

ZING Floor Coating & ZING Floor Coating + Plus are buffable finishes.

Use ZING Time Saver Hair Pad for all burnishing.

Use ZING CPC every time the floor is burnished.

Use ZING Floor Coating + Plus, with any 300 to 3,000 rpm electric, battery or propane machine.

Allow a minimum of 20-30 minutes drying time between coats.

Prior to recoating, use ZING Time Saver Hair Pad to open the pores & remove the dirt from the finish.

Keep from freezing.

Adhesive Coming Up Between Tiles Excessive or incorrect adhesive was used when tiles where installed. Remove the adhesive using ZING